Pull up the software and select the Pantone color needed, grab and weigh out colors specified in the formula, and mix. It’s that easy.
FN-INK™ is a non-phthalate, plastisol ink. If customers don’t need a Pantone color, you can use the ink right out of the bucket. FN-INK™ was designed by screen printers, for screen printers to be easy to work with. The FN-INK™ line includes 15-ready-to-use colors.
Bring your art to life with an endless amount of colors. Start mixing custom colors with the FN-INK™ Mixing System today.
FEATURES:
-
Bold and vibrant colors.
-
Creamy & Easy to Print Inks.
-
Soft hand prints.
-
Wet-on-wet printing.
-
Short flash times, lower cure temperature.
-
Printers can mix custom colors or use ink straight from the container.
FN-INK KIT INCLUDES:
-
FN-INK Mixing White
-
FN-INK Black
-
FN-INK Bright Red
-
FN-INK Ruby Red
-
FN-INK Yellow
-
FN-INK Golden Yellow
-
FN-INK Kelly Green
-
FN-INK Light Blue
-
FN-INK Royal Blue
-
FN-INK Light Royal Blue
-
FN-INK Navy Blue
-
FN-INK Magenta
-
FN-INK Fuchsia
-
FN-INK Orange
-
FN-INK Violet
Here's a breakdown for each kit:
Pint Kit: pint of all colors, quart of Mixing White
Quart Kit: pint of Magenta, gallon of Mixing White, quarts of remaining colors
Gallon Kit: quart of Magenta, five-gallon of Mixing White, gallons of remaining colors
DETAILS:
For single print colors, colors will reproduce best over white or light-colored garments. When printing on a base white, some color shifts may occur. This is normal and can be adjusted for by either printing a thicker ink deposit with lower mesh counts or by print-flash-print the color. You can also choose a slightly darker color in the PMS book. When it’s printed over the base white, it will typically lighten up and be a closer match. When direct printing over dark cotton, there is no guarantee you will maintain color integrity due to each ink's inherent opacity. As a result, not all colors will have good coverage when printed directly to fabric.
If printing a new PMS color, test through a 156 mesh onto white fabric, cure, and color checked in a light-corrected box, or light correct space. Printing onto mid- or dark-colored garments may require the use of a base white for best color reproduction. Since all PMS colors (across all ink mixing systems) vary in opacity and coverage, it’s recommended to test before running production.
MIXING INSTRUCTIONS:
To mix custom colors, you’ll also need a scale, spatulas, Pantone Coated Book, and mixing containers.
- Pull up the mixing software on your computer or phone.
- Type in the Pantone number or scroll through the drop-down menu.
- Input the amount of grams of ink you need in grams.
- Click “Load Formula.”
- On the left side of the screen, the formula will appear. It’ll show the colors needed and the amounts. On the right, a lightning bolt will show the Pantone color.
- Place the container onto the scale and zero it out.
- Start adding the ink with the highest volume listed in the formula.
- Once the appropriate amount is in the container, set that color aside and clean off the spatula with an ink cleaner like Supreme Wash. You can also use a spatula for each color to avoid contaminating the inks.
- Zero out the scale again and add the next highest volume. Repeat as necessary.
- Once all the colors have been added to the container, use a clean spatula to mix the ink. Be sure to scrape the ink from the bottom of the cup and mix it into the rest of the ink.
CURING INSTRUCTIONS:
Flash at 180-200°F, for 3 - 5 seconds. Each shop’s operating parameters might be faster or shorter depending on your production variable. Cure at 260°F, the ink is cured when it hits 260 throughout the entirety of the ink layer.
*Cure is attained when the ENTIRE ink layer reaches 260°, meaning that the ink is 260° from the top to the bottom of the ink layer. If you are using a laser gun to read the surface temp, this WILL be misleading. Laser temp guns give you a reflective reading. When tested side-by-side with a donut probe, you will see temperature differences as great as 120°-150° early in the cure cycle (the donut probe accurately measures the contact temperature where the crosshairs reside). As you reach the end of the dryer, those temperatures will get closer together. As a direct result – you will need to read a surface temp as little as 60° above what stated cure temp is and as much as 100° depending on how short your dryer tunnel is and how hot your settings are. This is due to a few things:
- The rate that plastisol ink absorbs heat. Some colors will heat up faster than others as they absorb infrared heat waves more readily.
- How hot the ink is when entering the tunnel. Cooler inks will take longer to heat up, thus taking longer to reach cure.
- The thickness of your ink deposit. As we all know, thicker ink deposits take longer to cure than thinner ink deposits. A longer dwell time is needed to reach full-cure through the whole ink layer. Heat/IR waves take time to penetrate and heat up the ink.
- The length of your tunnel. Curing ink is about temperature and time. It takes time for the entire ink layer to heat up and reach cure temp. The faster and hotter you run, the greater your chance to not reach full cure temp at the bottom of the ink layer.
- Cotton garments take longer to heat up compared to polyblends or 100% polyester. This is due to the absorptive nature of cotton. Cotton soaks up and holds onto water. When putting the shirt through the dryer, the dryer will release the water in the cotton fibers, slowing down how fast ink heats up. This process directly relates to how water based ink heats up and reaches cure, just on a smaller scale.
- The quality of your infrared panels. IR Panels are not created equal. Without diving into the deep details, some panels are more efficient in creating heat within the ink layer than others.
When changing your dryer to low cure temps, follow the recommendations and parameters laid out above and do wash testing to ensure your new dryer settings are reaching full cure.
CLEAN UP:
Ink degradent or press wash.
STORAGE INFORMATION:
Store at 65-90°F (18-32°C), avoiding direct sunlight. Ideal when used within one year of manufacturing date.